Hello Fred,
So I'm assuming you shook, then dumped all the catalyst in the catalyst bottle into the base, mixed, and poured. Is that correct? More questions ...
So was the whole thing sticky or partially set up? Or was part of it cured and part of it sticky/gooey? I'm assuming you've made molds where it cured fine and these are the only two you've had issues with? If so, do these two molds you've had issues with the same color pink as the ones that have cured properly? Or were they lighter or darker pink? Where did you get the High Strength 2? Did we ship it directly to you or did you purchase them through a retailer somewhere?
We will figure this out and get it straightened out for you.